Klassifikazzjoni tal-AWS: AWS 5.9
DESKRIZZJONI:
Il-wajer tal-iwweldjar tal-istainless steel għandu effiċjenza għolja ta' kisi, prestazzjoni teknika tajba tal-iwweldjar fl-iwweldjar f'kull pożizzjoni. Jintuża ħafna fl-industrija: struttura tal-bini, vetturi, inġinerija tal-pontijiet, makkinarju tal-minjieri, ferrovija, pajpijiet taż-żejt, tagħmir li jġorr il-pressjoni tal-gass, tagħmir tal-enerġija, eċċ.
NUMRU TAL-MUDELL U DAQS:
1. Servizz OEM tal-provvista tal-fabbrika.
2. Mudell: ER308 ER308L ER308LSi ER309 ER309L ER316 ER316L ER316LSi eċċ.
3. Daqs tal-wajer MIG: 0.8mm 0.9mm 1.0mm 1.2mm 1.6mm.
4. Daqs tal-wajer TIG: 1.6mm 2.0mm 2.4mm 3.2mm 4.0mm.
INTRODUZZJONI:
Nipprovdu tipi differenti ta' wajer tal-iwweldjar tal-istainless steel, inkluż wajer tal-iwweldjar solidu Mig, wajer tal-iwweldjar bil-vireg Tig u wajer tal-iwweldjar bl-ark mgħaddas, kollha ta' kwalità għolja u jinbiegħu mad-dinja kollha.
Minbarra 308 u 309, noffru wkoll 304, 321, 347, 316L, 310, 2209, u 201. Kif ukoll speċifikazzjonijiet speċjali bħal 318L, 904L, 2594, NiCrMo-3, Ni1.
IPPAKKJAR:
Ippakkjar tal-wajer tal-iwweldjar Mig (pakkett ta' rukkell u tanbur)
Dijametru: 0.8 - 2.0mm
Pakkett: 1 kg/rukkell, 5 kg/rukkell, 15 kg/rukkell, 20 kg/rukkell, 100 kg/tanbur, 200 kg/tanbur
Ippakkjar tal-wajer tal-iwweldjar bil-virga Tig (tubu tal-plastik)
Dijametru: 1.0 - 5.0mm
Pakkett: 5 kg/pakkett
Wajer tal-iwweldjar bl-ark mgħaddas
Dijametru: 2.5 - 5.0mm
Pakkett: 20kg/pakkett, 25 kg/pakkett
Ippakkjar newtrali u OEM huma milqugħa!
KOMPOŻIZZJONIJIET KIMIĊI TAL-WAJER TAL-IWELDER TAL-AZZAR INOSSIDABBLI:
| Numru tal-Mudell | C | Si | Mn | P | S | Cr | Ni | Mo | Cu |
| 304 | 0.08 | 0.30-1.00 | 2.00 | 0.045 | 0.030 | 18.00-20.00 | 8.00-11.00 | 0.18 | 0.003 |
| 304L | 0.03 | 0.30-1.00 | 2.00 | 0.045 | 0.030 | 18.00-20.00 | 8.00-12.00 | ||
| ER307 | 0.04-0.14 | 0.30-0.65 | 4.30-4.75 | 0.030 | 0.030 | 19.50-22.00 | 8.00-10.70 | 0.5-1.5 | 0.75 |
| ER308 | 0.08 | 0.30-0.65 | 4.30-4.75 | 0.030 | 0.030 | 19.50-22.00 | 9.00-11.00 | 0.75 | 0.75 |
| ER308L | 0.03 | 0.30-0.65 | 1.50-2.30 | 0.03 | 0.02 | 19.5-21.5 | 9.00-11.00 | 0.75 | 0.75 |
| ER308LSi | 0.03 | 0.65-1.00 | 1.60-2.40 | 0.03 | 0.02 | 19.5-21.5 | 9.0-11.0 | 0.75 | 0.75 |
| ER309 | 0.12 | 0.30-0.65 | 1.00-2.50 | 0.03 | 0.03 | 24.0-25.0 | 12.0-14.0 | 0.75 | 0.75 |
| ER309L | 0.03 | 0.3-0.65 | 1.5-2.3 | 0.03 | 0.02 | 23.0-25.0 | 12.0-14.0 | 0.75 | 0.75 |
| ER309LSi | 0.03 | 0.65-1.0 | 1.6-2.4 | 0.03 | 0.02 | 23.0-25.0 | 12.0-14.0 | 0.75 | 0.75 |
| ER316 | 0.08 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.03 | 18.00-12.00 | 11.0-14.0 | 2.0-3.0 | 0.75 |
| ER316L | 0.03 | 0.3-0.65 | 1.5-2.3 | 0.03 | 0.02 | 18.0-20.0 | 11.0-13.0 | 2.05-2.55 | 0.75 |
| ER316LSi | 0.03 | 0.65-1.0 | 1.6-2.4 | 0.03 | 0.02 | 18.0-20.0 | 11.0-13.0 | 2.05-2.55 | 0.75 |
| ER310 | 0.08-0.15 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.03 | 25.0-28.0 | 20.0-22.5 | 0.75 | 0.75 |
| ER347 | 0.08 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.03 | 19.0-21.5 | 9.0-11.0 | 0.75 | 0.75 |
| ER317 | 0.08 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.01 | 18.5-20.5 | 13.0-15.0 | 3.0-4.0 | 0.75 |
| ER321 | 0.08 | 0.3-0.65 | 1.5-2.5 | 0.03 | 0.01 | 18.5-20.5 | 9.0-10.5 | 0.75 | 0.75 |
| Numru tal-Mudell | Saħħa tat-tensjoni Rm (Mpa) | Saħħa tar-rendiment Rel jew Rp0.2 (Mpa) | Titwil (%) | Numru tal-Mudell | Saħħa tat-tensjoni Rm (Mpa) | Saħħa tar-rendiment Rel jew Rp0.2 (Mpa) | Titwil (%) |
| 304 | 550 | -- | 25 | ER309LSi | 510 | 320 | 25 |
| 304L | 510 | -- | 25 | ER316 | 510 | 320 | 25 |
| ER307 | 590 | 350 | 25 | ER316L | 510 | 320 | 25 |
| ER308 | 550 | 350 | 25 | ER316LSi | 510 | 320 | 20 |
| ER308L | 510 | 320 | 25 | ER310 | 550 | 350 | 25 |
| ER308LSi | 510 | 320 | 25 | ER347 | 550 | 350 | 25 |
| ER309 | 550 | 350 | 25 | ER317 | 550 | 350 | 25 |
| ER309L | 510 | 320 | 25 | ER321 | 550 | 350 | 25 |
| Kompożizzjoni tal-wajer tal-iwweldjar tal-istainless steel TIG u MIG | ||||||||||
| YB5092-2005 | AWS | Kompożizzjoni Kimika % | ||||||||
| C | Si | Mn | P | S | Cr | Ni | Mo | |||
| H08Cr20Ni9Mn7Si | ER307Si | 0.075 | 0.78 | 6.7 | 0.022 | 0.01 | 19.8 | 8.8 | ||
| H06Cr21Ni10 | ER308 | 0.045 | 0.45 | 1.9 | 0.02 | 0.009 | 20.8 | 9.8 | ||
| H0OCr21Ni10 | ER308L | 0.02 | 0.32 | 1.9 | 0.011 | 0.006 | 20 | 10.2 | ||
| H06Cr21Ni10Si | ER308Si | 0.045 | 0.85 | 1.5 | 0.022 | 0.01 | 20.8 | 9.8 | ||
| H06Cr24Ni13 | ER309 | 0.06 | 0.45 | 1.9 | 0.019 | 0.009 | 24.3 | 13.2 | ||
| H06Cr24Ni13Si | ER309Si | 0.06 | 0.79 | 1.95 | 0.019 | 0.009 | 24.7 | 13.2 | ||
| H03Cr24Ni13 | ER309L | 0.02 | 0.42 | 1.8 | 0.02 | 0.01 | 24.8 | 13.2 | ||
| H03Cr24Ni13Si | ER309LSi | 0.018 | 0.8 | 1.7 | 0.02 | 0.01 | 23.5 | 13.5 | ||
| H21Cr16Ni35 | ER330 | 0.2 | 0.38 | 1.5 | 0.022 | 0.01 | 16.5 | 34.5 | ||
| H06Cr19Ni12Mo2 | ER316 | 0.04 | 0.4 | 1.9 | 0.02 | 0.01 | 19.5 | 11.8 | 2.3 | |
| H06Cr19Ni12Mo2Si | ER316Si | 0.05 | 0.7 | 1.92 | 0.02 | 0.01 | 19.5 | 11.8 | 2.3 | |
| H03Cr19Ni12Mo2 | ER316L | 0.019 | 0.38 | 1.8 | 0.018 | 0.01 | 19.8 | 12.2 | 2.5 | |
| H03Cr19Ni12Mo2Si | ER316LSi | 0.06 | 0.85 | 1.7 | 0.022 | 0.01 | 18.8 | 12.6 | 2.4 | |
| H03Cr17Ni14Mo3 | ER317L | 0.02 | 0.38 | 1.8 | 0.02 | 0.01 | 18.8 | 13.8 | 3.6 | |
| H08Cr19Ni12Mo2Nb | ER318 | 0.06 | 0.42 | 1.5 | 0.022 | 0.01 | 18.5 | 11.8 | 2.3 | |
| H07Cr20Ni34Mo2Cu3Nb | ER320 | 0.06 | 0.4 | 1 | 0.022 | 0.01 | 19.8 | 33.3 | 2.8 | Nb0.7 |
| H02Cr20Ni34Mo2Cu3Nb | ER320L | 0.018 | 0.33 | 1.5 | 0.013 | 0.01 | 19.8 | 33.6 | 2.5 | Nb0.35 |
| H08Cr20Ni10Ti | ER321 | 0.06 | 0.45 | 1.5 | 0.022 | 0.01 | 20.8 | 9.8 | Ti9xC-1.0 | |
| H08Cr21 Ni10Nb | ER347 | 0.055 | 0.48 | 1.8 | 0.021 | 0.008 | 20.8 | 9.8 | Nb1xC-1.0 | |
| H12Cr26Ni21 | ER310 | 0.09 | 0.5 | 1.66 | 0.02 | 0.01 | 25.5 | 20.5 | ||
| H02Cr20Ni25Mo4Cu | ER385 | 0.02 | 0.3 | 1.5 | 0.018 | 0.01 | 20.2 | 24.8 | 4.8 | Cu 1.80 |
| H03Cr22Ni9Mo3N | ER2209 | 0.022 | 0.5 | 0.9 | 0.02 | 0.01 | 22.5 | 8.8 | 3.3 | N0.08-0.20 |
| H04Cr25Ni5Mo3Cu2N | ER2553 | 0.027 | 0.5 | 1 | 0.025 | 0.015 | 24.8 | 5.5 | 3.2 | N0.1-0.25 |
| H1 5Cr29Ni9 | ER312 | 0.09 | 0.38 | 1.5 | 0.022 | 0.01 | 29.5 | 8.5 | ||
| H03Cr24Ni13MoL | ER309L Mo | 0.023 | 0.45 | 1.5 | 0.022 | 0.01 | 23.8 | 13.2 | 2.2 | |
| H05Cr17Ni4Cu4Nb | ER630 | 0.04 | 0.39 | 0.5 | 0.022 | 0.01 | 16.5 | 4.8 | Cu;3 Nb;0.28 | |
| H08Cr26Ni5Mo2 | ER453s | 0.06 | 0.3 | 0.4 | 0.022 | 0.01 | 25.8 | 4.8 | 2.1 | |
| H08Cr21Ni10Mn6 | 0.06 | 0.35 | 5.5 | 0.022 | 0.01 | 20.8 | 9.8 | |||
| H05Cr22Ni11Mn6Mo3VN | ER209 | 0.04 | 0.4 | 4.5 | 0.022 | 0.01 | 21.5 | 10.8 | 2.2 | N;0.20 V;0.18 |
Wenzhou Tianyu Electronic Co., Ltd. twaqqfet fl-2000. Ilna involuti fil-manifattura ta' elettrodi tal-iwweldjar, vireg tal-iwweldjar, u konsumabbli tal-iwweldjar għal aktar minn 20 sena.
Il-prodotti ewlenin tagħna jinkludu elettrodi tal-iwweldjar tal-azzar li ma jissaddadx, elettrodi tal-iwweldjar tal-azzar tal-karbonju, elettrodi tal-iwweldjar b'liga baxxa, elettrodi tal-iwweldjar għall-wiċċ, elettrodi tal-iwweldjar b'liga tan-nikil u l-kobalt, wajers tal-iwweldjar tal-azzar ħafif u b'liga baxxa, wajers tal-iwweldjar tal-azzar li ma jissaddadx, wajers bil-qalba tal-fluss protetti bil-gass, wajers tal-iwweldjar tal-aluminju, wajers tal-iwweldjar bl-ark mgħaddas, wajers tal-iwweldjar b'liga tan-nikil u l-kobalt, wajers tal-iwweldjar tar-ram isfar, wajers tal-iwweldjar TIG u MIG, elettrodi tat-tungstenu, elettrodi tal-gouging tal-karbonju, u aċċessorji u konsumabbli oħra tal-iwweldjar.